OrcaSlicer config
This commit is contained in:
@@ -0,0 +1,54 @@
|
||||
{
|
||||
"type": "filament",
|
||||
"name": "Bambu ASA @base",
|
||||
"inherits": "fdm_filament_asa",
|
||||
"from": "system",
|
||||
"filament_id": "GFB01",
|
||||
"instantiation": "false",
|
||||
"description": "When printing this filament, there's a risk of warping and low layer adhesion strength. To get better results, please refer to this wiki: Printing Tips for High Temp / Engineering materials.",
|
||||
"eng_plate_temp": [
|
||||
"100"
|
||||
],
|
||||
"eng_plate_temp_initial_layer": [
|
||||
"100"
|
||||
],
|
||||
"fan_max_speed": [
|
||||
"35"
|
||||
],
|
||||
"filament_cost": [
|
||||
"31.99"
|
||||
],
|
||||
"filament_density": [
|
||||
"1.05"
|
||||
],
|
||||
"filament_flow_ratio": [
|
||||
"0.95"
|
||||
],
|
||||
"filament_max_volumetric_speed": [
|
||||
"12"
|
||||
],
|
||||
"filament_vendor": [
|
||||
"Bambu Lab"
|
||||
],
|
||||
"hot_plate_temp": [
|
||||
"100"
|
||||
],
|
||||
"hot_plate_temp_initial_layer": [
|
||||
"100"
|
||||
],
|
||||
"nozzle_temperature": [
|
||||
"270"
|
||||
],
|
||||
"nozzle_temperature_initial_layer": [
|
||||
"270"
|
||||
],
|
||||
"slow_down_layer_time": [
|
||||
"12"
|
||||
],
|
||||
"textured_plate_temp": [
|
||||
"100"
|
||||
],
|
||||
"textured_plate_temp_initial_layer": [
|
||||
"100"
|
||||
]
|
||||
}
|
||||
Reference in New Issue